Study links process defects to creep failure in PBF-LB 316L stainless steel
Researchers from Università Politecnica Delle Marche, Ancona, Italy, have published a study in the Journal of Materials Research investigating the short-term creep behaviour of AISI 316L stainless steel produced ... Read more »