APWorks introduces Scalmalloy 3% alloy with improved stress corrosion cracking resistance

MaterialsNews
November 20, 2026
APWorks’ Scalmalloy 3% aluminium alloy has been developed for Additive Manufacturing applications where resistance to stress corrosion cracking is a key consideration, including aerospace and defence (Courtesy APWorks)
APWorks’ Scalmalloy 3% aluminium alloy has been developed for Additive Manufacturing applications where resistance to stress corrosion cracking is a key consideration, including aerospace and defence (Courtesy APWorks)

APWorks, Taufkirchen, Germany, has introduced Scalmalloy 3%, a new variant of its Scalmalloy alloy family developed for applications where resistance to stress corrosion cracking (SCC) is an important material selection criterion. The 3% is in reference to the alloy’s magnesium content by weight.

According to the company, the alloy’s reduced magnesium content lowers its susceptibility to SCC under conditions that promote this form of cracking. The material is particularly suited to aerospace, defence and other structural applications exposed to demanding environmental conditions, where SCC resistance must be considered alongside strength, weight and Additive Manufacturing performance.

The introduction of Scalmalloy 3% expands the range of material properties available within the Scalmalloy family, providing structural engineers and service providers with an additional option to meet specific component requirements and operating conditions.

APWorks is inviting enquiries from engineers and service providers interested in evaluating Scalmalloy 3% for their applications or offering the material to customers.

www.apworks.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
November 20, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap