Velo3D selected for US Army metal AM award worth up to $10M

Velo3D, Inc., headquartered in Fremont, California, USA, has been selected by the US Army DEVCOM Armaments Center for an award potentially worth up to $10 million, subject to government funding of subsequent programme phases. The award comes under the Low-Cost Warheads and Lethal Payloads for Unmanned Systems challenge.
The programme is intended to accelerate the transition of commercial technologies into defence applications, drawing on Velo3D’s expertise in advanced metal Additive Manufacturing.
“This award demonstrates the role advanced manufacturing can play in strengthening the U.S. defence industrial base,” said Arun Jeldi, CEO, Velo3D. “Our technology and manufacturing expertise can help the Government evaluate new materials, produce complex components and establish repeatable production processes for critical defence applications.”

Under the programme, Velo3D will use Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing to produce components that may be difficult or uneconomical to manufacture using conventional methods. The work will progress through process development, initial hardware production, Government testing and refinement, followed by a low-rate initial production demonstration.
The project will focus on two material pathways: Inconel 718, for which Velo3D has an established process qualified on its Sapphire platform, and a second, Government-directed high-performance alloy for which an Additive Manufacturing process will be developed and qualified.
Velo3D will be responsible for Additive Manufacturing process development, production, inspection and quality documentation. The Government will retain design authority and responsibility for lethality, ballistic, functional and performance testing.

The programme also includes development of a Technology Transition Package documenting manufacturing processes, quality requirements and production procedures. The package will support repeatable production at qualified domestic manufacturing facilities.
“Velo3D’s technology and scale hold a lot of promise for bringing new capabilities to the Warfighter,” added Dan Suarez, Research Engineer, U.S. Army DEVCOM Armaments Center.