Additive Manufacturing of highly-stressed components in hardened martensitic stainless steel
The Institute of Production Engineering and Machine Tools (IFW), part of the Hannover University’s engineering centre (PZH) in Garbsen, Germany, and the Fraunhofer Institute for Additive Manufacturing Technologies ... Read more »