GranuDrum method formalised in ASTM D8648-25 standard
GranuTools, based in Awans, Belgium, has announced that its GranuDrum powder characterisation technology is now covered by a new ASTM standard: ASTM D8648-25 – Standard Test Method for Determining ... Read more »