Fraunhofer and MacLean-Fogg develop AM process for large HPDC molds for automotive sector
Researchers from Fraunhofer ILT, Aachen, Germany, and MacLean-Fogg, Mundelein, Illinois, USA, have successfully demonstrated a scalable process for the Additive Manufacturing of large aluminium components ... Read more »