In-situ X-ray imaging reveals PBF-EB melt pool dynamics

NewsResearch
September 22, 2025
Experimental setup at the P61A beamline with the MiniMelt in-situ PBF-EB system mounted on a heavy-load diffractometer, the high-speed X-ray imaging system and an indication of the X-ray beam path (Courtesy Additive Manufacturing)
Experimental setup at the P61A beamline with the MiniMelt in-situ PBF-EB system mounted on a heavy-load diffractometer, the high-speed X-ray imaging system and an indication of the X-ray beam path (Courtesy Additive Manufacturing)

Researchers from German institutions Friedrich-Alexander-Universität, Erlangen-Nürnberg, and Institute of Materials Physics, Geesthact and Sweden’s KTH Royal Institute of Technology, Stockholm, have published a paper in Additive Manufacturing focused on the use of in-situ imaging in Electron Beam Powder Bed Fusion (PBF-EB) Additive Manufacturing.

Despite the technology’s ability to process materials at >1000°C, a limited fundamental understanding of the intricate dynamics and melt pool formation has seen advanced processing strategies largely confined to experimental parameter studies. This has been because numerical models have mostly been unable to accurately predict processing conditions at the part or layer scale. In ‘In-situ synchrotron imaging of powder consolidation and melt pool dynamics in electron beam powder bed fusion’, the researchers performed high-speed in-situ X-ray imaging during multi-layer single track powder melting experiments on MiniMelt (a recently developed, custom-built PBF-EB machine for in-situ X-ray investigations).

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The paper noted several key melt pool formation dynamics, some of which the researchers state have been noticed for the first time. The imaging shows how melt pool formation involves the coalescence of molten powder particles into larger droplets and how these droplets either fuse with the melt pool or solidify as balling particles. Results are also said to elucidate the origins of melt pool oscillations and spatter formation and demonstrate how the superposition of the combined effect of these mechanisms can lead to chaotic and escalating movement within the melt.

In the abstract, the researchers noted, “We expect our results to improve and extend the phenomenological understanding of the powder consolidation mechanisms during PBF-EB and to aid in the development of new scanning strategies as well as the validation of numerical models.”

‘In-situ synchrotron imaging of powder consolidation and melt pool dynamics in electron beam powder bed fusion’ is available here.

www.fau.eu

www.hereon.de

www.kth.se

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
NewsResearch
September 22, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap