Chemically reduced tungsten powder achieves 99.9% density in PBF-EB

MaterialsNewsResearch
September 17, 2025
Scanning Electron Microscope image of chemically reduced tungsten powder. The powder exhibits a faceted morphology and is non-flowable according to ASTM B213
Scanning Electron Microscope image of chemically reduced tungsten powder. The powder exhibits a faceted morphology and is non-flowable according to ASTM B213

Freemelt AB, based in Mölndal, Sweden, has announced that researchers have processed chemically reduced tungsten into dense material (99.8-99.9%) using a Freemelt ONE Electron Beam Powder Bed Fusion (PBF-EB) Additive Manufacturing machine. This breakthrough, reported in a new open-access paper by Mid Sweden University, UPC Barcelona, Sandvik, Wolfram, and Freemelt, demonstrates the potential for use in high-temperature applications across defence, energy, and MedTech industries.

The study introduced an approach for optimising process development in PBF-EB of non-flowing chemically reduced tungsten powder. Both line- and spot melting strategies were employed, with gradient-based variations of key processing parameters such as beam current and scanning speed (for line melting) and dwell time (for spot melting) applied across both XZ and XY planes using prismatic test specimens. This method allowed for the mapping of the transition from porous to swelling material within a single specimen and exposed the effects of changing gradient directions.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Scripts were developed to analyse swelling and porosity from stacked backscattered electron data, providing insights into material density and defect distribution. Optimal parameters for line melting (1400 W, 115 mm/s) and spot melting (1400 W, 4.5 ms dwell time) were identified, resulting in high-density samples.

Solid samples with densities of 99.8% and 99.9% as measured by the Archimedes method were achieved. Microscopical analysis verified parameter windows with dense, swelling-free material, selected for further builds and detailed characterisation. Microstructural and compositional analysis was conducted using SEM and EBSD, while local micromechanical properties were assessed through microhardness. Scaling of line melting was deemed infeasible due to warping, while spot melting was scaled to a melting area of 50 mm × 50 mm.

The full article, ‘PBF-EB process development of chemically reduced tungsten via a dual-gradient parameter approach utilizing the backscatter signal’ by William Sjöström, Stefan Roos, Carlos Botero, and Lars-Erik Rännar, Mid Sweden University; Lei Zhu and Emilio Jimenez-Pique, Universitat Politècnica de Catalunya; and Arun Balachandramurthi, Freemelt, is available here.

freemelt.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
September 17, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap