Research shows potential of EHLA in rapid alloy development
Researchers from the RWTH Aachen Chair for Digital Additive Production (DAP), RWTH Aachen University, Germany, have investigated the feasibility of using Extreme High-Speed Laser Material Deposition ... Read more »