HP and Hyperion partner to expand tungsten carbide Additive Manufacturing

HP Metal Jet S100 Binder Jetting (BJT) machine, the model installed at Hyperion's production facility near Barcelona in October 2026 for tungsten carbide Additive Manufacturing using CarbiForm powders (Courtesy Hyperion Materials & Technologies)
HP Metal Jet S100 Binder Jetting (BJT) machine, the model installed at Hyperion’s production facility near Barcelona in October 2026 for tungsten carbide Additive Manufacturing using CarbiForm powders (Courtesy Hyperion Materials & Technologies)

HP Additive Manufacturing (HP), based in Sant Cugat del Vallès, Spain, and Hyperion Materials & Technologies, Worthington, Ohio, USA, have announced a Strategic Preferred Partner Agreement aimed at expanding the commercial use of tungsten carbide (WC) Additive Manufacturing. The companies intend to make rapid prototyping and production-ready WC components more accessible to industrial customers worldwide.

In October 2026, Hyperion installed a new HP Metal Jet S100 machine at its production facility in Barcelona. The collaboration combines HP’s Binder Jetting (BJT) Additive Manufacturing machine with Hyperion’s expertise in WC manufacturing, sintering and finishing. The companies state that this will provide a route from application development and qualification through to serial production.

The process uses Hyperion’s new CarbiForm range of ready-to-use tungsten carbide powders, developed specifically for BJT Additive Manufacturing. The powders have been tested for use with HP Metal Jet printers in conjunction with Hyperion’s sintering operations.

“This preferred partner agreement allows us to combine our decades of hard-materials experience with HP’s highly scalable Additive Manufacturing platform,” stated Biju Varghese, Chief Technology Officer at Hyperion. “The result is a new manufacturing option for customers looking to create complex, high-performance tungsten carbide components and bring them to production with confidence.”

According to the companies, the collaboration could enable manufacturers to produce complex geometries, application-specific features, consolidated components and customised solutions that may be difficult or uneconomical to manufacture using conventional methods. They also identify opportunities to shorten development cycles and improve material utilisation while maintaining the performance characteristics of tungsten carbide required for demanding industrial applications.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

“Hyperion brings the depth of expertise needed to help scale WC Additive Manufacturing on HP Metal Jet printers,” said Arvind Rangarajan, Head of Product & Strategy at HP Additive Manufacturing. “Its knowledge across the tungsten carbide value chain, combined with HP’s technology, can help customers translate the design freedom of Additive Manufacturing into reliable, production-ready components.”

With commercial manufacturing capability now available through Hyperion using its HP Metal Jet S100 machine, the companies plan to work jointly with customers to identify and qualify applications where tungsten carbide Additive Manufacturing could offer technical and economic advantages.

www.hp.com

www.hyperionmt.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap