FIT joins HP Metal Jet manufacturing partner network

FIT Additive Manufacturing Group, headquartered in Lupburg, Germany, has been named a new manufacturing partner for HP Metal Jet, HP’s metal Binder Jetting (BJT) technology. FIT is set to offer contract manufacturing services using the technology.
At a recent joint FIT and HP workshop, the companies explored Binder Jetting’s positioning relative to Laser Beam Powder Bed Fusion (PBF-LB), Metal Injection Moulding (MIM) and conventional manufacturing. Topics included materials, design guidelines, applications and total cost of ownership (TCO).

The companies also discussed how Binder Jetting could be applied to customer projects and scaled for industrial production.
Founded in 1995, FIT has over thirty years of experience in Additive Manufacturing, producing prototypes, tooling, individual parts, series components, spare parts and works of art.