6K Additive reports 72% growth in metal powder revenue in Q3 2026

6K Additive offers US-produced materials for Additive Manufacturing (Courtesy of 6K Additive)
6K Additive offers US-produced materials for Additive Manufacturing (Courtesy of 6K Additive)

6K Additive, Inc., based in Burgettstown, Pennsylvania, USA, has reported growing demand for its metal powders in its quarterly activities report for the period ended 30 September 2026. Powder order intake increased 43% quarter-on-quarter to $12.3 million, while powder revenue rose 72% year-on-year to $5.5 million.

The company manufactures metal powders for Additive Manufacturing and alloy additions for the aluminium industry. Its UniMelt technology converts revert materials, including used powder, into spherical metal powders such as titanium, nickel and refractory metals.

Nickel powder revenue increased 50% quarter-on-quarter, driven by demand from defence customers, contract manufacturers and Original Equipment Manufacturers (OEMs). The company’s total order backlog reached $18.1 million, up 52% from the previous quarter.

During Q3, 6K Additive secured a long-term supply agreement with Addman, covering a 30-month programme for Alloy 718 powder valued at between $8.1 million and $10.8 million. The agreement includes dedicated stocking support and closed-loop revert recycling.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The company also reported progress on its manufacturing capacity expansion in Burgettstown, where the precast structure housing its UniMelt bays is nearing completion. Initial commissioning of the powder expansion is expected in late Q4 2026, with production ramp-up planned for Q1 2027.Following the quarter, 6K Additive finalised a $27.4 million loan agreement with the Export-Import Bank of the United States (EXIM) to support the expansion of its US manufacturing operations.

www.6kadditive.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap