Hexagon named CADS Additive software reseller
Software provider CADS Additive GmbH, Perg, Austria, has named Swedish group Hexagon as a distribution partner in over 100 countries. Through this partnership, Hexagon anticipates the ability to better meet its customers ... Read more »