Mitsubishi Electric US and Novineer are evaluating NoviVision's AI-powered photo-based reconstruction technology for DED repair, with initial tests demonstrating faster geometry capture than conventional 3D scanning (Courtesy Mitsubishi Electric US/Novineer)
Mitsubishi Electric US and Novineer are evaluating NoviVision’s AI-powered photo-based reconstruction technology for DED repair, with the initial test demonstrating faster geometry capture than conventional 3D scanning (Courtesy Mitsubishi Electric US/Novineer)

Mitsubishi Electric US, Cypress, California, and Novineer, Daytona Beach, Florida, are jointly evaluating NoviVision, an AI-powered photo-based reconstruction platform, for reverse engineering in Directed Energy Deposition (DED) repair applications using Mitsubishi Electric’s AZ600 wire-laser DED Additive Manufacturing system.

In a first single-sample evaluation, NoviVision reconstructed a 292 mm-high twisted-blade sample from smartphone photographs in 5–10 minutes, compared with 30–45 minutes for conventional 3D scanning. The reconstructed model achieved a root-mean-square error (RMSE) of 0.818 mm against a 3D-scanner reference.

The evaluation aims to establish whether photo-based reconstruction can provide sufficient geometric accuracy for DED repair without specialist scanning equipment. The twisted-blade sample was selected because its curved, non-prismatic geometry presents a greater reconstruction challenge than simpler components such as blocks or brackets.

As DED produces near-net-shape components that are subsequently finish-machined to achieve the required dimensional tolerances, the reconstructed CAD model does not necessarily need scanner-grade accuracy. Instead, it must represent the geometry sufficiently to guide material deposition while leaving adequate material for machining.

Physical twisted-blade sample used in the NoviVision reconstruction evaluation (Courtesy Mitsubishi Electric US/Novineer)
Physical twisted-blade sample used in the NoviVision reconstruction evaluation (Courtesy Mitsubishi Electric US/Novineer)

Photo-based reconstruction process

NoviVision generates 3D models from photographs taken at multiple angles using a standard smartphone, without requiring calibration markers, fixtures or specialist capture equipment. The images are uploaded to a cloud-based or privately installed version of the platform and processed using AI to generate STL and STEP files. The STEP output can be used in CAD, CAM or robotic workflows.

For the evaluation, photographs of the completed twisted-blade build were captured from four directions – front, back, left and right – and processed to generate a STEP file. The same component was measured using a Creality Raptor Pro 3D scanner, which required calibration markers to be attached before scanning.

Evaluation results

The NoviVision reconstruction was compared with the 3D-scanner data, which was considered the closest available benchmark rather than an absolute ground truth, as the scanner’s calibration markers can introduce small measurement differences.

Workflow comparison: NoviVision photo capture (5–10 min) versus the 3D-scanner method (30–45 min), step by step (Courtesy Mitsubishi Electric US/Novineer)
Workflow comparison: NoviVision photo capture (5–10 min) versus the 3D-scanner method (30–45 min), step by step (Courtesy Mitsubishi Electric US/Novineer)

The comparison found an RMSE of 0.818 mm between the NoviVision STEP model and the scanner reference, with a mean absolute error of 0.628 mm and a standard deviation of 0.811 mm.

By comparison, the difference between the reference scan and the original design CAD was approximately 3.35 mm RMSE, reflecting the intentional dimensional allowance of a near-net-shape DED component produced oversize for subsequent machining, rather than a manufacturing defect.

This difference is approximately four times the reconstruction error of 0.818 mm, suggesting that photo-based reconstruction could provide sufficient accuracy for certain repair operations. However, the figures represent different geometric comparisons and do not, on their own, establish suitability for a particular repair tolerance.

NoviVision's reconstruction error (0.82 mm RMSE) is approximately four times smaller than the difference between the original design CAD and the as-built component (3.35 mm RMSE) (Courtesy Mitsubishi Electric US/Novineer)
NoviVision’s reconstruction error (0.82 mm RMSE) is approximately four times smaller than the difference between the original design CAD and the as-built component (3.35 mm RMSE) (Courtesy Mitsubishi Electric US/Novineer)

All comparison values were calculated against the 3D-scanner reference and rescaled to a 293.23 mm diagonal basis. Any mean bias relative to the scanner reflects the reconstruction process rather than manufacturing deposition error.

The evaluation also identified variations in reconstruction accuracy. Deviations were relatively small in regions adequately covered by photographs but increased in areas with limited image coverage, particularly top surfaces and shadowed regions.

With the current four-view capture arrangement, the largest local deviations occurred at the top vertex. Approximately 95% of measured points were within 1.46 mm of the reference, although a small number approached 2 mm. Novineer is working to improve reconstruction accuracy and robustness in top-facing and partially obscured regions.

Signed surface-deviation distribution across the twisted-blade sample (NoviVision reconstruction vs scanner reference). Deviations are smallest on faces the four input photographs cover well and grow on top and shadowed surfaces — the warm band along the trailing edge and top vertex marks the largest local differences (Courtesy Mitsubishi Electric US/Novineer)
Signed surface-deviation distribution across the twisted-blade sample (NoviVision reconstruction vs scanner reference). Deviations are smallest on faces the four input photographs cover well and grow on top and shadowed surfaces — the warm band along the trailing edge and top vertex marks the largest local differences (Courtesy Mitsubishi Electric US/Novineer)
Accuracy summary, NoviVision reconstruction vs 3D-scanner reference. All values compared with the 3D-scanner reference (Creality Raptor Pro). Rescaled to 293.23 mm diagonal basis. Scanner treated as reference, not ground truth. Mean bias is a property of the reconstruction pipeline relative to the scanner - not a direct measure of manufacturing deposition error (Courtesy Mitsubishi Electric US/Novineer)
Accuracy summary, NoviVision reconstruction vs 3D-scanner reference. All values compared with the 3D-scanner reference (Creality Raptor Pro). Rescaled to 293.23 mm diagonal basis. Scanner treated as reference, not ground truth. Mean bias is a property of the reconstruction pipeline relative to the scanner – not a direct measure of manufacturing deposition error (Courtesy Mitsubishi Electric US/Novineer)

Potential applications

The companies have identified three potential applications for photo-based geometry capture, with reverse engineering for repair the primary focus of the current evaluation.

For mold and die repair or component restoration, an operator could photograph a worn component, generate a CAD model and use the resulting geometry to plan a DED cladding toolpath. Following deposition, the component would be finish-machined to the required tolerances. This could reduce the time and equipment needed for geometry capture where scanner-level accuracy is unnecessary.

Another potential application is component reconstruction at remote facilities, customer sites or locations where dedicated scanning equipment is unavailable or impractical to deploy. Smartphone capture and access to a cloud-based or private processing environment could enable reverse engineering without transporting specialist scanning hardware.

Looking further ahead, photo-based reconstruction could support in-process geometry checks during DED builds. Capturing geometry at intervals could help operators monitor dimensional changes and determine whether intervention is necessary. However, this would require further improvements in reconstruction accuracy and integration with the manufacturing system.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Further evaluation

“In our evaluation, NoviVision produced a usable digital model from standard photographs in a fraction of the time a scanner-based workflow requires,” stated Takashi Kai, Strategy Manager, Mitsubishi Electric US. “For repair workflows, where final accuracy is set by finish machining, this kind of fast, low-friction geometry capture is a direction we think is worth evaluating further with Novineer.”

According to Novineer, NoviVision’s relative reconstruction error remains approximately stable as part size increases, potentially offering a more favourable accuracy-to-size relationship for larger components. However, this has yet to be validated through the joint evaluation. As larger components can also be more challenging to measure using conventional scanners, faster photo-based capture could offer additional benefits.

Mitsubishi Electric US and Novineer plan to extend the evaluation to additional samples covering a wider range of component sizes and geometries. Further work will examine improvements to image coverage, reconstruction robustness and CAD-output capabilities.

The companies intend to use the findings to establish which DED Additive Manufacturing repair applications could benefit from photo-based reconstruction and where conventional measurement methods remain necessary.

us.mitsubishielectric.com

novineer.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNewsSoftware
November 23, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap