Desktop Metal and Uniformity Labs announce new aluminium powder for use in Binder Jetting
Through a collaboration between Desktop Metal, Burlington, Massachusetts, USA, and Uniformity Labs, Fremont, California, a new powder enabling aluminium sintering for Binder Jetting (BJT) AM technology ... Read more »