Fabrisonic’s ultrasonic Additive Manufacturing used to produce aluminium satellite heat exchangers
Fabrisonic LLC, a manufacturer of Ultrasonic Additive Manufacturing (UAM) solutions, headquartered in Columbus, Ohio, USA, has utilised its SonicLayer® 1200 metal Additive Manufacturing machine ... Read more »