Fehrmann’s AlMgty brings colour to additively manufactured parts
Fehrmann Alloys GmbH & Co KG, Hamburg, Germany, has reported that its silicon-free aluminium alloy AlMgty has the ability to be anodised in a variety of colours, bringing the option to its metal ... Read more »