O’Shaughnessy Ventures awards $100K to Michelle Wang for additively manufactured magnet research
Investment firm O’Shaughnessy Ventures LLC, has awarded an O’Shaughnessy Fellowship to Michelle Wang, an engineer based in New York based on her work developing additively manufactured magnets. ... Read more »