EPMA publishes Euro PM2021 technical programme
The European Powder Metallurgy Association (EPMA) has published the full technical programme for Euro PM2021, scheduled to take place virtually on October 18–22, 2021. The scope of the conference covers all aspects of PM ... Read more »