ICAM 2021 releases preliminary conference programme
The 2021 ASTM International Conference on Additive Manufacturing (ICAM 2021) has released a preliminary programme. Sponsored by the ASTM International Additive Manufacturing Center of Excellence, ICAM 2021 is scheduled to take place November 1–5, 2021, in Anaheim, California, USA.
ICAM 2021 will be held both in-person and virtually. Virtual attendance includes pre-recorded presentations, as well as live-streamed keynote speeches and panel sessions.
The five-day conference will include nearly 600 presentations, including more than 240 invited and 120 student presentations. It will also feature ten panel sessions and several keynote addresses. Before the conference, on October 31, four in-person certificate short courses will be held, covering an array of Additive Manufacturing topics.
ICAM 2021 will also include presentations of the ASTM International Young Professional in Additive Manufacturing Awards and the Awards of Excellence. Award nominations from the public are welcome.
Over the years, ICAM has grown to be the largest ASTM International scientific conference. This event involves numerous ASTM technical committees and external stakeholders, bringing experts from all around the world to exchange the latest developments in the field of AM with an emphasis on research to applications through standardisation.
Further information is available through the event’s website.