HiETA’s Bristol locations host four Renishaw AM machines and post-processing facilities (Courtesy HiETA)

Working with British chemical propulsion developer Protolaunch, HiETA Technologies, Bristol, UK, has additively manufactured the combustion chamber and nozzle for the company’s reusable 10kN HILBERT rocket engine. This engine acts as a testbed to test and validate key performance metrics that underpin the thermodynamic cycle under development by Protolaunch, which aims to eliminate the need for complex turbomachinery.

Protolaunch develops rocket engines for small launch applications; as a company, they also work with the European Space Agency and international launch partners to scale up and tailor propulsion solutions ready for launch. The company realised the potential of AM to reduce the part count of its overall system and enable complex internal flow paths within the parts themselves. It required two large parts with complex internal geometry and challenging wall thickness requirements to be produced at short notice.

The team of engineers at HiETA were able to advise and make the necessary design adjustments to allow these parts to benefit from the Additive Manufacturing process. HiETA’s two sites in Bristol offer a comprehensive range of machines, including four Renishaw RenAM 500Q AM machines, coupled with post-processing facilities which offered the flexibility and capability to give Protolaunch the speed and experience needed to meet its tight deadline as well as quality expectations.

www.hieta.biz

www.protolaunch.co.uk

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap