A life cycle assessment confirms that CHIPART's recycling method has the potential to reduce CO2 emissions by between 85-92% compared to the use of virgin titanium powder (Courtesy Danish Technological Institute)
A life cycle assessment confirms that CHIPART’s recycling method has the potential to reduce CO2 emissions by between 85-92% compared to the use of virgin titanium powder (Courtesy Danish Technological Institute)

The Danish Technological Institute, together with project partners IDONIAL of Spain and CRM Group of Belgium, is presenting the results of the recently completed CHIPART (Chips to Parts: Circularity of Titanium Scrap from Machining to Additive Manufacturing) project to the European Defence Agency (EDA) in Liège.

Supported by the EDA, the twelve-month proof-of-concept project investigated the potential to reduce the environmental impact and costs associated with titanium powder production. The analysis also indicated that total manufacturing costs, including machine time and post-processing, could be lower than when using only virgin titanium powder. According to the researchers, the project has demonstrated that titanium machining chips from the aerospace industry can be converted into metal powder suitable for Additive Manufacturing without the need for remelting.

“By converting machining chips directly into metal powder for Additive Manufacturing without remelting, we have shown that circularity in titanium manufacturing can provide environmental benefits and be economically viable on a large scale,” stated Magdalena Müller, materials specialist at the Danish Technological Institute.

The recycled titanium powder was evaluated using two metal AM processes: Laser Beam Powder Bed Fusion (PBF-LB) and Directed Energy Deposition (DED).

“We found that mixing recycled powder with new titanium powder produced the best results, and that controlling the oxygen level in the machine was the decisive factor for print quality,” Müller explained.

Following optimisation of the process parameters, the project achieved a reported material density of at least 98% in the manufactured parts, meeting its target.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The Danish Technological Institute also developed an economic model based on a demonstrator component to assess the potential costs of using recycled powder. Although recycling costs were higher at laboratory scale, the model indicated that industrial-scale production could deliver recycled titanium powder at a significantly lower cost than virgin powder.

The analysis also suggested that overall manufacturing costs could be reduced when machine time and post-processing were taken into account, compared with manufacturing using only virgin titanium powder.

CHIPART ran from October 2025 to September 2026 under the Incubation Forum for Circular Economy in European Defence (IF CEED). The project involved additional industrial partners from the aerospace and defence sectors, which supplied titanium machining chips and a reference demonstrator component.

The project builds on the earlier VARETIT initiative, which also involved the Danish Technological Institute and investigated recycling titanium scrap into powder for Additive Manufacturing.

www.dti.dk

www.idonial.com

www.crmgroup.be

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
October 13, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap