Addireen’s green-laser Additive Manufacturing technology achieves 99.9% dense pure copper parts
A joint research team from Shanghai Jiao Tong University and Shanghai University has published a paper focusing on the use of green lasers in processing copper via Laser Beam Powder Bed Fusion (PBF-LB) ... Read more »