ORNL additively manufactures defect-free tungsten components
Researchers at Oak Ridge National Laboratory (ORNL), Oak Ridge, Tennessee, USA, are reported to have used electron beam Additive Manufacturing to produce defect-free, complex tungsten parts, suitable for use in extreme ... Read more »