Research collaboration develops advanced copper Additive Manufacturing process for heat sink design
ToffeeX, London, UK, in collaboration with Imperial College London and the University of Wolverhampton, has developed a design framework that brings multiscale analysis to physics-driven design. At the point ... Read more »