Rapidia launches new rapid cooling furnace
Sinter-based Additive Manufacturing technology developer Rapidia Inc, based in Vancouver, British Columbia, Canada, has launched a new rapid cooling furnace ... Read more »
Sinter-based Additive Manufacturing technology developer Rapidia Inc, based in Vancouver, British Columbia, Canada, has launched a new rapid cooling furnace ... Read more »
Blue Power Casting Systems GmbH, Walzbachtal, Germany, in cooperation with Amazemet Sp. z o. o., a Warsaw University of Technology spin-off company, have developed a compact ultrasonic atomisation ... Read more »
3D Systems Corporation, Rock Hill, South Carolina, USA, reports that it has achieved significant progress in the creation of what it states is the world’s largest, fastest, most precise powder metal Additive Manufacturing ... Read more »
Micromeritics Instrument Corporation, Norcross, Georgia, USA, a supplier of high-performance systems used to characterise particles, powders and porous materials, reports that its fully automated Micromeritics ... Read more »
The winners of the international purmundus challenge 2020, which ran with the theme Geometry and Material in Harmony, have been announced in a prize-giving event at Formnext Connect ... Read more »
Castor Technologies Ltd, Tel Aviv, Israel, has launched CASTOR Enterprise, a proprietary software which is said to enable manufacturers to automatically reduce costs, by utilising the benefits ... Read more »
Epson Atmix Corporation, Aomori, Japan, an Epson Group company, has begun operations on a new production line at its Kita-Inter Plant, Hachinohe, Japan. Built with an investment of approximately ... Read more »
Desktop Metal, Burlington, Massachusetts, USA, has officially launched Live Sinter™, a software solution designed to eliminate the trial and error required to achieve high-accuracy parts using sinter-based metal powder ... Read more »
Independent commercial testing laboratory NSL Analytical Services, Inc., Cleveland, Ohio, USA, has posted a number of videos in its online ‘Tech Talk’ series which feature presentations, conversations and demonstrations ... Read more »
SLM Solutions Group AG, Lübeck, Germany, has officially launched its new SLM® machine, the NXG XII 600, which is now available for commercial offer. The Laser Beam Powder Bed Fusion (PBF-LB) ... Read more »
Sintavia LLC, Hollywood, Florida, USA, reports that it has achieved ISO 14001 approval for the environmental management system at its Hollywood location. The new accreditation, which is issued ... Read more »
Metal Additive Manufacturing technology company 3DEO, Los Angeles, California, USA, has won a Gold Medal in Additive Manufacturing from Design World’s Leadership in Engineering Achievement Program ... Read more »