Rio Tinto opens new Canadian scandium plant
Rio Tinto has begun production of high-quality scandium oxide at a new commercial scale demonstration plant at its Rio Tinto Fer et Titane (RTFT) metallurgical complex in Sorel-Tracy, Quebec, Canada ... Read more »