IFT Vienna advances hybrid manufacturing with breakthrough in Ad-Proc-Add II project combining additive and subtractive technologies

Exemplary build strategies for large-volume component geometries, illustrated using a modified handle segment. The geometry was adapted for the DED process (Courtesy TU Wien)
Exemplary build strategies for large-volume component geometries, illustrated using a modified handle segment. The geometry was adapted for the DED process (Courtesy TU Wien)

As part of the international research project Ad-Proc-Add II (Advanced Processing of Additively Manufactured Parts II), the Institute of Production Engineering and Photonic Technologies (IFT) at TU Wien, Vienna, Austria, is contributing to the advancement of hybrid manufacturing processes. In close collaboration with partner institutions from Austria, Germany, and Belgium, IFT has developed innovative approaches for combining additive and subtractive methods along the entire process chain.

The project, funded by the Austrian Research Promotion Agency (FFG), the German Federal Ministry for Economic Affairs and Climate Action (BMWK), and for Flanders Agency for Innovation & Entrepreneurship (VLAIO), was coordinated by the ecoplus Mechatronics Cluster, FKM, and KU Leuven. Its goal was to enhance the cost-efficiency and precision of manufacturing highly complex components. In this context, IFT played a key role in developing innovative, application-ready technological solutions using simulation-based process models, which are expected to make future industrial applications significantly more efficient and sustainable.

Materials and process knowledge for DED components

One of IFT’s research priorities was analysing the resulting material structure and surface integrity along the Additive-Subtractive Manufacturing (ASM) process chain. In the area of Directed Energy Deposition (DED), researchers in Vienna examined, among other factors, the influence of various process parameters and post-processing methods on surface and substructure properties. The findings provide crucial insights for the targeted adjustment of component characteristics such as hardness, residual stresses, and surface roughness.

Machine Hammer Peening, an intermediate treatment method tested by IFT, demonstrated significant improvements in the densification and homogenisation of the surfaces of additively manufactured components. When combined with methods such as shot peening and Hirtisation, post-processing could be systematically optimised.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Simulation as a bridge between Additive and Subtractive Manufacturing

A key contribution from IFT was the development of a simulation model to predict the topography, stress distribution, and deformation of additively manufactured components even before the actual production process begins. Using the Finite Element Method (FEM), a foundation was established for predictive process planning.

In a further step, the simulation was extended to include an analysis of machinability, with the aim of optimising machining strategies in advance based on the AM data. This enables precise definition of the minimum necessary machining allowances, significantly reducing material consumption and post-processing time.

Hybrid CAM systems and process data databases

IFT also developed a prototype of a CAM rule engine to support the digital integration of the ASM process chain. This enables the automated adjustment of toolpaths based on sensor-driven process data. The system was embedded into a custom-developed cross-process database that links parameters and sensor data from various stages of manufacturing. This brings the vision of a fully data-driven process chain within reach.

Key role for small and medium-sized enterprises (SMEs)

IFT placed particular emphasis on industrial applicability, especially for small and medium-sized enterprises (SMEs). By strategically combining research, simulation, and practical validation, usable solutions were developed in collaboration with 15 Austrian industry partners, including approaches for the seamless integration of DED processes into existing production lines. This resulted in practical, cost-effective, and scalable technologies.

Strong international collaboration

The Ad-Proc-Add II project was coordinated by the Research Association for Mechanical Engineering e.V. (FKM) and supported by renowned institutions such as the Institute for Machine Tools (IfW) at the University of Stuttgart and the Institute for Machining Technology (ISF) at TU Dortmund University. IFT, with its interdisciplinary team led by Univ.-Prof. Dipl.-Ing. Dr.techn. habil. Friedrich Bleicher, played a central role in the project.

The research findings are being shared through professional events, trade fairs, and publications.

www.ad-proc-add.eu

www.tuwien.at

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap