Continuum Powders introduces CFR for small-batch and speciality alloys

Custom Foundry Runtime gives access to Continuum’s advanced plasma-gas atomisation platform for speciality alloy development, small-batch production, and high-value material processing (Courtesy Continuum Powders)
Custom Foundry Runtime gives access to Continuum’s advanced plasma-gas atomisation platform for speciality alloy development, small-batch production, and high-value material processing (Courtesy Continuum Powders)

Continuum Powders, based in Houston, Texas, USA, has launched Custom Foundry Runtime (CFR), a new service that offers manufacturers, researchers, and advanced materials developers flexible access to Continuum’s advanced plasma-gas atomisation platform for speciality alloy development, small-batch production, and high-value material processing.

BLT Inside The World’s Largest Metal Additive Manufacturing Parts Production Operation

While Continuum continues to supply production-scale titanium and nickel for advanced manufacturing applications, the company says its roots have always been deeply connected to speciality alloy development and metallurgical innovation.

CFR provides a scalable, customer-facing service designed to solve a growing challenge in the market: the lack of accessible, secure, and economically viable pathways for processing small-volume, high-value materials.

Across aerospace, medical, energy, and defence, organisations are increasingly working with specialised alloys, proprietary chemistries, and precious metals that are difficult to process through traditional foundry or atomisation providers due to minimum volume requirements, production economics, or material sensitivity.

“Custom Foundry Runtime represents an important evolution for Continuum Powders,” stated Jon Cozens, CEO. “We’re seeing growing demand for flexible alloy development and secure processing capabilities, particularly for customers working with highly specialised or precious materials. CFR gives companies access to advanced atomisation infrastructure without forcing them into traditional large-scale production models that don’t fit their needs.”

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The programme enables customers to:

  • Develop and validate new alloy chemistries
  • Process small-batch and speciality metal runs (as low as 40-50 kg)
  • Atomise high-value or precious metal materials, including platinum group metal (PGM) alloys and gold-based materials (400 OTN/day)
  • Support rapid R&D and qualification programs
  • Scale from development quantities into commercial production
  • Maintain tighter oversight of proprietary or sensitive materials

CFR is supported by Continuum’s metallurgical knowledge, advanced process controls, and secure material handling protocols designed specifically for high-value feedstocks and speciality alloys.

The new service offering is designed for agile development programs, pilot-scale initiatives, and strategic materials projects where speed, flexibility, and technical collaboration are essential. The result is said to be a more efficient path from concept to production that supports both material innovation and supply chain resilience.

Discover more about Custom Foundry Runtime here.

continuumpowders.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap