Renault Trucks: Metal Additive Manufacturing could reduce engine weight by 25%
A team of Renault Trucks engineers and designers is looking at metal Additive Manufacturing to boost the performance of its engines. The Renault Trucks Lyon Powertrain Engineering department ... Read more »