Optomec adds 7000 series aluminium to its list of qualified alloys
Optomec Inc, Albuquerque, New Mexico, USA, has added 7000 series aluminium to its growing list of qualified alloys for use in its LENS metal Directed Energy Deposition (DED) ... Read more »