Oerlikon introduces alloy to replace super duplex stainless steels
At Formnext 2021, Oerlikon AM, Pfäffikon, Schwyz, Switzerland, is presenting a new alloy to match the strength and corrosion resistance of super duplex stainless steels (DSS) ... Read more »