Nordic AM Alliance launched to strengthen regional cooperation

The Nordic Quantum Alliance was launched during the IQT Nordics conference at Oslo Metropolitan University (Courtesy Nordic Quantum Alliance)
The Nordic Quantum Alliance was launched during the IQT Nordics conference at Oslo Metropolitan University (Courtesy Nordic Quantum Alliance)

The Nordic Additive Manufacturing Alliance (NAMA) has been established to bring together leading Additive Manufacturing organisations from Finland, Sweden, Norway and Denmark in what the member organisations have described as the first coordinated Nordic collaboration network focused on the technology.

Supported under Nordic Innovation’s Nordic Forward: Competitiveness and Resilience for 2050 programme, the initiative aims to strengthen sustainable manufacturing, improve supply chain resilience and support industrial innovation across the Nordic region.

The project comes amid growing interest in more flexible and sustainable production models as manufacturers seek to address supply chain disruptions, decarbonisation targets and increasing digitalisation requirements.

Additive Manufacturing is increasingly adopted as a means of enabling localised, on-demand production while reducing material consumption and inventory requirements. While the Nordic countries have established expertise in the technology, collaboration between national ecosystems has remained limited.

“The Nordic countries already have world-class expertise in Additive Manufacturing, but it remains fragmented across different actors and countries,” stated Eetu Holstein, Senior Ecosystem Lead of the FAME Ecosystem at DIMECC Ltd. “Through NAMA, we are building Nordic cooperation that strengthens industrial resilience, accelerates sustainable manufacturing, and gives the Nordic region a stronger common voice internationally.”

The alliance brings together Finland’s FAME – Finnish Additive Manufacturing Ecosystem, Sweden’s RISE Research Institutes of Sweden, the Norwegian Additive Manufacturing Cluster and Denmark’s Danish AM Hub.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

According to the project partners, each participating country contributes complementary expertise. Sweden is recognised for materials development and metal powder production; Finland for industrial implementation and digital design; Denmark for circular business models and innovation ecosystems; and Norway for applications in the maritime and energy sectors.

Running from 2026 to 2028, the project will map Additive Manufacturing capabilities across the Nordic region, identify industrial requirements, develop a shared governance framework and establish a long-term roadmap for regional cooperation.

The initiative also seeks to strengthen Nordic participation in the future development of European and international manufacturing strategies.

“Through the Nordic AM Alliance, we are strengthening the Nordic region’s long-term competitiveness and resilience,” stated Sindre Bornstein, Managing Director of Nordic Innovation. “Additive Manufacturing is a critical technology for sustainability, digitalisation and innovation, with each Nordic country holding complementary strengths. By bringing these strengths together, we can speed up the green transition and enhance industrial resilience across borders.”

NAMA is one of seven projects selected for funding under Nordic Innovation’s Green and Competitive Nordic Region call, which forms part of the wider Nordic Forward: Competitiveness and Resilience for 2050 programme.

www.nordicinnovation.org

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap