AP&C installs two new atomisation reactors
Arcam AB has announced that its metal powder subsidiary AP&C, based in Montreal, Canada, is building its fourth and fifth reactors, adding significant capacity to its titanium and nickel super-alloy powder manufacturing operation. ... Read more »