JEOL, NC State and ORNL test PBF-EB tungsten tiles in fusion device

NC State nuclear engineering undergraduate Olivia Mehalick inside the DIII-D vacuum vessel during installation of the 3D-printed tungsten tiles (Courtesy North Carolina State University, Oak Ridge National Laboratory (ORNL) and JEOL)
NC State nuclear engineering undergraduate Olivia Mehalick inside the DIII-D vacuum vessel during installation of the 3D-printed tungsten tiles (Courtesy North Carolina State University, Oak Ridge National Laboratory (ORNL) and JEOL)

North Carolina State University (NC State); Oak Ridge National Laboratory (ORNL), Tennessee, USA; and JEOL Ltd, headquartered in Akishima, Tokyo, have additively manufactured full-size tungsten tiles for the lower divertor of the DIII-D fusion device. At the DIII-D National Fusion Facility in San Diego, the tile surfaces were exposed to plasma discharges with significant heat and particle flux, and came through intact.

From invitation to installed hardware in approximately eight months, the project was born out of NC State’s research partnership with DIII-D National Fusion Facility, bringing together three groups with expertise in Electron Beam Powder Bed Fusion (PBF-EB) and tungsten Additive Manufacturing. JEOL’s large-format PBF-EB machine, JAM-5200EBM, was used to manufacture the full-size tiles.

“We appreciate the opportunity to collaborate with NC State, ORNL, and General Atomics, on a project that brings together advanced materials research, fusion science, and JEOL’s long-standing expertise in precisely controlled electron beam technologies,” said Tom Isabell, President of JEOL USA. “Producing full-size tungsten tiles for DIII-D is exactly the kind of challenge our JAM-5200EBM system was designed to address. By applying our optics, beam-control, and Additive Manufacturing expertise alongside outstanding partners, we are helping demonstrate a practical path toward the complex, high-performance components future fusion systems will require.”

Finished flat and domed tungsten tiles with mirror-like plasma-facing surfaces, ready for installation in DIII-D (Courtesy North Carolina State University, Oak Ridge National Laboratory (ORNL) and JEOL)
Finished flat and domed tungsten tiles with mirror-like plasma-facing surfaces, ready for installation in DIII-D (Courtesy North Carolina State University, Oak Ridge National Laboratory (ORNL) and JEOL)

Divertor tiles in ITER and future fusion power plants are expected to withstand steady heat loads of 10–20 MW/m², with brief bursts reaching substantially higher levels, tungsten is considered a leading candidate material, with the highest melting point of any metal, 3,422°C. Each tile pair measures approximately 136 by 143 mm and 20 mm thick.

“Tungsten is currently the material everyone wants in a fusion reactor, but it is extremely difficult to manufacture into complex shapes,” said Dr Michael Kirka, ORNL. “We were able to do this with electron beam Additive Manufacturing, when most of the field thought printed tungsten would always crack. These tiles are the payoff from years of that work.”

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Wire Electrical Discharge Machining (EDM) was used to shape the mounting features and a gently domed surface with a radius of about 1 m. A multi-axis CNC grinder, programmed with a digital twin of the tile, then removed about 250 microns from the plasma-facing surface. The tiles were mounted on copper-alloy pedestals and installed in DIII-D’s lower divertor in July 2026. During a three-day testing campaign, they experienced 74 high-confinement plasma discharges at medium-to-high power, totalling approximately four minutes of plasma exposure.

The tiles are now being removed, imaged and surface-scanned to compare with their condition before exposure, prior to returning to NC State for further analysis.

“DIII-D lets us put candidate materials in front of a real fusion plasma and see what happens,” stated Dr Chris Ledford, ORNL. “Seeing additively manufactured tungsten go from small test buttons to full-size tiles in the divertor in less than a year is remarkable, and the data from this campaign will help guide how tungsten components are designed for ITER and beyond.”

www.jeolusa.com

www.ncsu.edu

www.ornl.gov

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap