Expansion of HIP and vacuum heat treatment capabilities at ITS Bilbao

EquipmentNews
October 25, 2024
ITS Bilbao has announced an expansion of its Hot Isostatic Pressing and vacuum heat treatment capabilities (Courtesy ITS Bilbao)
ITS Bilbao has announced an expansion of its Hot Isostatic Pressing and vacuum heat treatment capabilities (Courtesy ITS Bilbao)

Isostatic Toll Services Bilbao SL (ITS Bilbao), Spain, has announced that it intends to commission its fourth MEGA Hot Isostatic Pressing (HIP) unit within the next three years and, by Q2 2025, to commission a fully molybdenum vacuum heat treatment furnace from TAV. Its first heat treatment unit, the 1200 x 1600 x 1200 mm furnace will feature a maximum vacuum of 10-5 mbar, making it suitable for titanium. This additional heat treatment capability will enable ITS Bilbao to offer a combined MEGA HIP and MEGA Heat Treatment service to its HIP customers.

BLT Inside The World’s Largest Metal Additive Manufacturing Parts Production Operation

ITS Bilbao ran the first cycle of its MEGA HIP unit in December 2019. While the COVID-19 pandemic followed shortly after, with its impact on the aerospace sector felt by the company, demand for toll HIP services surged again following the recovery. This increased demand prompted the company to decide, in Q1 2022, to double its existing capacity. A MEGA HIP unit, identical to the original, was commissioned in the following year.

Over the following twelve months, demand for the second unit exceeded its capacity, leading to the installation of a third MEGA HIP unit in 2024. Set to be commissioned in 2025, the unit is identical to the previous, with a Ø1088 x 2570 mm loadable zone corresponding to 2.4 m3, and an increased maximum working pressure of up to 138 MPa (20,000 psi).

www.isostatictollservices.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
EquipmentNews
October 25, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap