GKN PM identifies dual-phase steel powder for industrial auto applications in IDAM project
As the Industrialization and Digitalization of Additive Manufacturing (IDAM) project reaches its halfway stage, GKN Powder Metallurgy, one of the twelve project partners, reports it has identified its new DP 600 ... Read more »