GKN Aerospace and USAF launch TITAN-AM for aerostructures
GKN Aerospace has announced the launch of TITAN-AM (Titanium Industrialisation and Technology Advancement for Near-net Additive Manufacturing), an $8.4 million programme in partnership with the US Air Force ... Read more »