QuesTek collaborates with Aubert & Duval to accelerate predictive alloy development
QuesTek Innovations LLC, Evanston, Illinois, USA, recently highlighted its collaboration with Aubert & Duval (A&D) to accelerate alloy development using predictive composition modelling. By simulating material ... Read more »