Aurora Labs produces its first metal powders for Additive Manufacturing
Aurora Labs Ltd, Bibra Lake, Western Australia, has produced the first batch of laboratory test-scale powder from its prototype powder production unit (PPU). According to the company, the prototype PPU ... Read more »