APWORKS qualifies Farsoon FS422M for Scalmalloy production

EquipmentMaterialsNews
November 12, 2024
APWORKS has qualified the Farsoon FS422M for Scalmalloy production (Courtesy Farsoon Europe GmbH)
APWORKS has qualified the Farsoon FS422M for Scalmalloy production (Courtesy Farsoon Europe GmbH)

APWORKS, based in Taufkirchen, Germany, has announced that Scalmalloy, an aluminium-scandium alloy known for its high strength-to-weight ratio and exceptional corrosion resistance, is now qualified for use on the Farsoon FS422M metal Additive Manufacturing machine.

Scalmalloy is recognised as the material of choice for sectors requiring lightweight, high-strength, and corrosion-resistant components, such as aerospace, automotive, and robotics.

BLT Inside The World’s Largest Metal Additive Manufacturing Parts Production Operation

“Qualifying the Farsoon FS422M for Scalmalloy represents a significant milestone,” stated Jon Meyer, CEO at APWORKS. “This achievement enables us to deliver even greater value to our customers through higher rate of production, and also allows us to produce larger size parts. We have been impressed by the mechanical properties achieved on the Farsoon system which are consistently in the upper quartile of the tensile strength we have seen across the many different powder bed fusion systems we have qualified Scalmalloy on.” 

 Qualified Scalmalloy production data (Courtesy APWORKS)
Qualified Scalmalloy production data (Courtesy APWORKS)

The Farsoon FS422M is reported to offer manufacturers high-precision capabilities and scalability. It allows the production of parts that meet stringent quality standards while optimising production costs. Qualifying this machine for Scalmalloy parts represents a leap forward in both technological compatibility and material performance.

“We’re thrilled to advance metal Additive Manufacturing with the FS422M’s qualification for Scalmalloy parts together with APWORKS,” stated Oliver Li, Managing Director of Farsoon Europe. “This milestone not only demonstrates the machine’s exceptional precision and scalability but also opens up new possibilities for high-performance applications in various industries.”

APWORKS will showcase the latest applications of Scalmalloy at the Farsoon Europe booth 11.0-E11 at Formnext 2024.

www.farsoon.com

www.apworks.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
EquipmentMaterialsNews
November 12, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap