US Air Force employs Phase3D to develop real-time Additive Manufacturing inspection

Phase3D has developed a real-time inspection and certification technology for powder-based Additive Manufacturing (Courtesy Phase3D)
Phase3D has developed a real-time inspection and certification technology for powder-based Additive Manufacturing (Courtesy Phase3D)

Phase3D, a startup based in Chicago, Illinois, USA, has been selected by the US Air Force to further Additive Manufacturing quality inspection through a Phase I contract from the Air Force Research Lab (AFRL) and the Small Business Technology Transfer (STTR) programme. In collaboration with the University of Dayton Research Institute (UDRI), Phase3D intends to propel the development of Fringe Research, a real-time inspection and certification technology for powder-based Additive Manufacturing.

Specifically, this contract focuses on combining data from multiple sensors to improve defect detection. Phase3D’s focus is to advance flaw detection and part quality assurance for critical use Additive Manufacturing applications.

“Phase3D’s heightmap data does not exist in a vacuum. While we have seen excellent correlation and predictive capabilities from heightmap layer data from structured light, we are excited to announce the development of incorporating multiple data streams to increase detection capabilities to our customers,” Dr Niall O’Dowd, founder and CEO of Phase3D, shared.

This collaborative effort between Phase3D, the US Air Force, and UDRI is said to represent a crucial step forward for the AM industry. By integrating data from multiple sensors, Phase3D’s technology works to enhance the accuracy and reliability of in-situ monitoring, paving the way for early detection look of part defects and enabling interventions during the build process. This can include repairs or stopping the build outright, reducing scrap rates and improving overall yield.

The impact of this development on the AM industry is hoper to extend beyond the immediate benefits to the aerospace industry. By reducing scrap rates and improving build quality inspection, Fringe Research from Phase3D may help customers reduce project lead times, increase machine utilisation, and ensure build quality.

www.phase-3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap