Gefertec launches arc80X Wire Arc Additive Manufacturing machine

EquipmentNews
March 7, 2024
The modularity of the arc80X WAAM machine allows customers to create a bespoke system (Courtesy Gefertec)
The modularity of the arc80X WAAM machine allows customers to create a bespoke system (Courtesy Gefertec)

Gefertec GmbH, Berlin, Germany, has announced its new arc80X Wire Arc Additive Manufacturing (WAAM) machine is now available.

The arc80X’s modular design offers a selection of welding systems from a variety of manufacturers, allowing customers to design a machine suited to their requirements. This flexibility also allows it to be upgraded or converted if customers wish to implement new functions.

The arc80X features automated tool measurement, gas nozzle cleaning, wire cutting and the replacement of wear parts. These functionalities are reported to increase efficiency and reduce manual effort.

Integrated process monitors records and stores all relevant data during the build process. This allows for comprehensive documentation for quality assurance and process optimisation. Additionally, the pyrometer integrated into the arc80X and the active component cooling enables reliable and efficient temperature management of the part.

Adjustable automatic routines react to ignition failures during the production process and keep it running. In addition, the titanium module enables the manufacture of components in a closed inert gas atmosphere, which is essential for the processing of sensitive materials.

The arc80X offers a wide range of table options, from five-axis simultaneous machining to 3+2 to pure three-axis machining. Customers can determine the capabilities of their machines according to the needs of their parts.

www.gefertec.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
EquipmentNews
March 7, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap