Daegun Tech’s AM impeller completes 18 months in nuclear plant

ApplicationsNews
October 8, 2026
The additively manufactured stainless steel impeller, produced by Daegun Tech using PBF-LB (Courtesy Daegun Tech)
The additively manufactured stainless steel impeller, produced by Daegun Tech using PBF-LB (Courtesy Daegun Tech)

Daegun Tech, a manufacturer of metal Additive Manufacturing machines and components based in Changwon, South Korea, has reported that an impeller it produced for Unit 1 of the Saeul Nuclear Power Plant has successfully completed eighteen months of operation.

Developed in collaboration with Korea Hydro & Nuclear Power (KHNP) and other South Korean companies, the multi-blade 316L stainless steel impeller was manufactured by Daegun Tech using one of its internally developed Laser Beam Powder Bed Fusion (PBF-LB) AM machines.

The impeller is used in the cooling system for the plant’s generator circuit breaker. Unlike conventional designs, which comprise blades assembled onto a fixed plate with potentially vulnerable joints, the new impeller integrates the blades and plate into a single component.

The additively manufactured impeller is used in the cooling system for the plant's generator circuit breaker (Courtesy Daegun Tech)
The additively manufactured impeller is used in the cooling system for the plant’s generator circuit breaker (Courtesy Daegun Tech)

Following heat treatment, mechanical property testing and airflow testing, the impeller was installed in January 2025 and reportedly operated without problems until scheduled preventive maintenance in July 2026.

The project used South Korean design, manufacturing and testing capabilities to replace previously imported components. KHNP now plans to expand the use of Additive Manufacturing to other nuclear power plants and is considering applications in Small Modular Reactors (SMRs).

“The future market for metal 3D printing lies in the integration and weight reduction of precision industrial parts, which are difficult to achieve with conventional manufacturing methods,” stated Ki Soo Shin, CEO of Daegun Tech. “Based on our track record in the nuclear power generation field, we will expand our application to high value-added industries that require high reliability, such as defence, aerospace, and energy.”

www.daeguntech.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
October 8, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap