Sciaky highlights large-scale electron beam metal AM technology at Formnext 2026

Sciaky, Inc., based in Chicago, Illinois, USA, is highlighting its Electron Beam Additive Manufacturing (EBAM) technology, a wire-fed form of Directed Energy Deposition (DED), at Formnext 2026 in Frankfurt, Germany.
The company is exhibiting alongside Evobeam GmbH, Mainz, Germany, with which it has collaborated since 2013. Evobeam specialises in electron beam and laser-based Additive Manufacturing and welding under vacuum, including technologies for processing refractory metals.
Sciaky’s EBAM process uses an electron beam to melt wire feedstock, depositing metal layer by layer to produce near-net-shape components for subsequent heat treatment and finish machining.

Designed for large-scale metal AM, Sciaky’s EBAM machines offer work envelopes up to 5.79 × 1.22 × 1.22 m, with the capability to produce round parts up to 2.44 m in diameter. The technology can also accommodate smaller components, starting at approximately 203 mm (8 in).
Gross deposition rates range from 3.18–18.14 kg/h, depending on the material and part geometry. In 2022, Sciaky reported that France’s Saint Exupéry Institute for Research in Technology (IRT) had achieved a titanium deposition rate of 18.14 kg/h during its Metallic Advanced Materials for Aeronautics (MAMA) project.
EBAM incorporates Sciaky’s Interlayer Real-time Imaging and Sensing System (IRISS), a patented closed-loop control technology that monitors deposition and automatically adjusts electron beam power, wire feed rates and CNC motion profiles. According to Sciaky, this helps maintain consistency in part geometry, mechanical properties, microstructure and metal chemistry, while recording process data for traceability.

The technology has been used in aerospace applications, including the production of titanium satellite fuel tank components by Lockheed Martin Space. In 2018, Sciaky reported that its EBAM process had achieved qualification following testing of 1.17 m diameter titanium fuel tank domes. The company stated that production time had been reduced by 87%, with delivery times falling from two years to three months.
More recently, in June 2026, Sciaky announced a partnership with NX Atomics to apply EBAM to the production of components for its small modular reactor platform.
Suitable materials include titanium alloys, nickel-based superalloys, stainless steels and refractory metals such as tantalum, tungsten and niobium. Sciaky also offers dual-wire feed configurations, allowing different alloys to be combined within a single melt pool to produce custom compositions and compositionally graded structures.
According to Sciaky, EBAM can reduce material waste, shorten lead times and cut machining time by up to 80% compared with conventional manufacturing. The vacuum-based process also eliminates the need for inert shielding gases.
Sciaky offers EBAM machines and contract manufacturing services for prototypes, production components, repair and remanufacturing applications.
Sciaky is exhibiting at Formnext in Hall 11.0, Booth F52.