AI framework improves defect detection in AM alloys

A graphical abstract of the development of the AI framework for defect detection (Courtesy https://doi.org/10.1016/j.actamat.2026.122101)
A graphical abstract of the development of the AI framework for defect detection (Courtesy https://doi.org/10.1016/j.actamat.2026.122101)

Researchers from South Korean organisations Pohang University of Science and Technology (POSTECH), Korea Institute of Materials Science (KIMS), and the Hyundai Motor Group, and the Japanese University of Osaka have published research in Acta Materialia detailing their development of an AI framework to detect defects in additively manufactured materials.

Chanel: When manufacturing process becomes part of luxury value

The yield strength of alloys manufactured via Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing remains difficult to predict due to defect-driven variability that cannot be captured by conventional near-dense empirical equations. In ‘Data-selective machine learning framework (DSML) for defect-aware, interpretable yield-strength prediction for LPBF-fabricated AlSi10Mg alloys’, the authors developed a data-selective machine learning (DSML) pipeline that integrates data-driven black-box modelling with physics-informed white-box modelling through symbolic regression, enabling the derivation of a defect-aware, interpretable closed-form equation.

A dual-source dataset was constructed, comprising forty-four fully labelled datasets – including process parameters, microstructural features and mechanical properties – alongside 111 process-only datasets containing porosity data. The DSML framework identifies key descriptors and incorporates a porosity sub-model into a closed-form yield-strength equation, explicitly accounting for the influence of process-induced defects.

Validation was conducted using AlSi10Mg produced by PBF-LB Additive Manufacturing under six distinct conditions. Results indicate that the porosity-aware white-box model achieves a coefficient of determination of 0.90 and a mean absolute error (MAE) of 9.51 MPa, outperforming both the black-box model and a widely used cell-size-based empirical relation (MAE = 41.98 MPa).

Steel reinvented: Colnago’s Steelnovo and the search for the perfect modern road bike

The derived terms are consistent with established mechanisms, including effective load-bearing reduction due to pores and boundary-mediated strengthening, while maintaining dimensional consistency. This enables the development of process–design maps for defect-aware optimisation.

By incorporating defect effects into an interpretable equation and validating against independent experimental conditions, the researchers noted that their study presents a reproducible, physics-consistent approach to understanding process–structure–property relationships in AM AlSi10Mg, and provides a scalable framework for integrating additional strengthening mechanisms in future Laser Beam Powder Bed Fusion materials.

The paper is available here.

www.postech.ac.kr

www.kims.re.kr

www.hyundaimotorgroup.com

www.osaka-u.ac.jp

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap