Farsoon and Tekna collaborate to industrialise coarse Ti64 for PBF-LB

Farsoon and Tekna have extended their collaboration to support the industrialisation of coarse Ti-6Al-4V powders in Additive Manufacturing (Courtesy Tekna)
Farsoon and Tekna have extended their collaboration to support the industrialisation of coarse Ti-6Al-4V powders in Additive Manufacturing (Courtesy Tekna)

Farsoon Europe GmbH, based in Sindelfingen, Germany, has extended its collaboration with Tekna Holding ASA, headquartered in Sherbrooke, Quebec, Canada, to support the industrialisation of coarse Ti-6Al-4V powders in Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing. The development addresses market demand for increased productivity, improved powder handling, safety and reduced cost per part.

Farsoon’s open-platform approach enables users to extend process parameters beyond conventional limits. By combining coarse powder with thicker layer deposition, the companies report that build times can be reduced while maintaining process stability.

Tekna’s plasma atomisation technology enables the production of both coarse and fine powder fractions from the same source. This allows users to qualify multiple process strategies more efficiently, reducing material approval requirements and lowering overall industrialisation costs.

Fine powders typically used in PBF-LB Additive Manufacturing, however, are often classified as flammable and can require complex safety measures which increases operational costs. Tekna’s coarse Ti64 powder (TEKMAT Ti64-90/45) is said to offer lower oxygen sensitivity, enabling safer handling, recycling, storage and transport. This supports industrial-scale deployment by reducing both risk and cost throughout the powder lifecycle.

To highlight the compatibility between Tekna’s plasma-atomised powders and Farsoon’s open platform technology, titanium components were successfully produced using Tekna’s TEKMAT™ Ti64-53/20-G23 powder on the Farsoon FS721M-H-8-CAMS AM machine (Courtesy Farsoon Technologies)
To highlight the compatibility between Tekna’s plasma-atomised powders and Farsoon’s open platform technology, titanium components were successfully produced using Tekna’s TEKMAT™ Ti64-53/20-G23 powder on the Farsoon FS721M-H-8-CAMS AM machine (Courtesy Farsoon Technologies)

Testing on the FS273M-2 and FS721M-H-8-CAMS systems at a 90 μm layer thickness has shown that, despite the increased layer thickness, as-built Ti-6Al-4V mechanical properties remain aligned with standard PBF-LB benchmarks. These include yield strength of ≥ 850 MPa and ultimate tensile strength of ≥ 900 MPa.

Compared to a typical 60 μm layer thickness, the theoretical build rate increases by more than 20%, contributing to higher machine productivity and lower manufacturing costs.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Shaped-beam technology for increased throughput

Farsoon is further developing its process capability through shaped beam technology, moving beyond conventional Gaussian beam exposure. Shaped beams enable larger and adjustable spot sizes, customised energy distribution and improved melt pool stability at increased layer thicknesses.

This approach is reported to support the reliable processing of coarse powders and enables a significant increase in productivity. By combining thicker layers with shaped beam exposure, the theoretical build rate per laser can increase by more than 80% compared to processing at 90 μm with a Gaussian beam.

The company states that shaped beam technology is a key enabler for series and mass production, supporting the transition of PBF-LB from prototype-focused applications to economically viable serial production.

www.tekna.com

www.farsoon.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap