Divergent’s Additive Manufacturing is based around its Divergent Adaptive Production System, using PB-LB and robotic assembly (Courtesy Divergent Technologies)
Divergent’s Additive Manufacturing is based around its Divergent Adaptive Production System, using PB-LB and robotic assembly (Courtesy Divergent Technologies)

Divergent Technologies, based in Torrance, California, USA, reports it has been formally qualified for Additive Manufacturing US Army ground vehicle parts through the Complex AM Assembly Printing Pilot CRADA with the US Army DEVCOM Ground Vehicle Systems Center (GVSC).

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Divergent’s Additive Manufacturing is based around its Divergent Adaptive Production System (DAPS™), an end-to-end structural engineering design and manufacturing process that leverages AI-driven design, Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing, and robotic assembly.

“This qualification validates our Additive Manufacturing process for mission-critical hardware and marks another step toward software-defined manufacturing at scale for defence,” the company stated on LinkedIn.

The US Army DEVCOM GVSC is the US Army’s research and development centre for advanced ground vehicle technologies. The engineers, scientists, technicians, and project leaders at GVSC support the Army’s ground vehicles beginning with basic research in support of the future of ground vehicle technology, further developing emerging technologies for integration onto Army platforms, sustaining platforms through their lifecycles, and all of the research, development, testing, integration, and relationship building with our industry partners that is necessary to be successful in providing its Warfighters with the best capabilities possible.

www.divergent3d.com

gvsc.devcom.army.mil

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

ApplicationsNews
February 10, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap