Anyuan Mold adds UnionTech metal AM machines for custom footwear moulds

Anyuan Mold, a leading footwear mould manufacturer headquartered in Shanghai, China, has added two Fuees430 four-laser metal Additive Manufacturing machines from UnionTech, also located in Shanghai.

Since its establishment in 2020, Anyuan Mold has specialised in the footwear mould sector, placing technological innovation at its core. The company is reported to have conducted year-long market research and equipment testing in its search for a metal AM technology partner, resulting in the purchase of two UnionTech Fuees430 Laser Beam Powder Bed Fusion (PBF-LB) AM machines.

Anyuan Mold and UnionTech stated they intend to continue their cooperation, exploring more possibilities in the metal additively manufactured footwear mould sector, promoting the development of China’s footwear industry and supporting the broader goal of strengthening its presence in global high-end manufacturing.