Wallwork to highlight expanded HIP capacity at Formnext

Wallwork operates two Quintus Technologies HIP systems at its Manchester facility (Courtesy Wallwork)
Wallwork operates two Quintus Technologies HIP systems at its Manchester facility (Courtesy Wallwork)

Wallwork Group, based in Bury, UK, will highlight its expanded Hot Isostatic Pressing (HIP) capacity at Formnext 2026, following a £20 million investment in its HIP Centre.

The company now operates two Quintus Technologies HIP systems at its Manchester facility. The second machine, commissioned in late 2025, doubled the site’s HIP capacity and is intended to support customers in Additive Manufacturing, casting and Powder Metallurgy.

“Over the last three years we have moved from establishing a new UK HIP facility to operating two of Europe’s most advanced Quintus systems and supporting customers in the UK, Europe and beyond,” stated Howard Maher, Wallwork Group Sales Manager.

The two identical machines enable processing to be transferred between units, with interchangeable tooling and continuity of service during scheduled maintenance.

Both systems operate at pressures of 40–207 MPa (5,800–30,000 psi) and temperatures up to 1250 °C. They also incorporate Quintus Technologies’ Uniform Rapid Cooling technology for controlled cooling within the HIP cycle.

Wallwork Group also operates more than thirty vacuum furnaces, enabling HIP and heat treatment to be incorporated within a wider range of thermal processing services. The company offers standard, shared and bespoke HIP cycles.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

“Formnext brings together many engineers who are pushing the limits of Additive Manufacturing, castings and Powder Metallurgy. Applying high temperature and isostatic gas pressure densifies components and reduces internal defects. This helps engineers achieve the material properties and consistency demanded in safety-critical and high-value applications. Wallwork has the technology, capacity, quality systems and technical expertise to support the transition from product development into scaled-up reliable production,” added Maher.

The HIP Centre holds Nadcap and AS9100 accreditation. Across four UK sites, Wallwork Group also provides heat treatment, vacuum brazing and PVD coating services.

Wallwork will exhibit at Formnext 2026 in Hall 11, Booth F35.

www.wallworkht.co.uk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap